• We’re currently investigating an issue related to the forum theme and styling that is impacting page layout and visual formatting. The problem has been identified, and we are actively working on a resolution. There is no impact to user data or functionality, this is strictly a front-end display issue. We’ll post an update once the fix has been deployed. Thanks for your patience while we get this sorted.

Arctic Silver 3

Maverick2002

Diamond Member
I got one of these tubes as an engineering sample and reviewed it. After retesting I still got the same results. Like 4C (load) and 1-2C (idle) drop with the thermal material as the ONLY different factor. Wow. Hehe you guys gotta wait til end of January to get it 😀
 
If you look on the graph you'll see that the drops are in comparison to Alumina which has pretty much identical performance to AS2.

John: I already posted in the other thread.
 
If you look on the graph you'll see that the drops are in comparison to Alumina which has pretty much identical performance to AS2.

Doh! I'm in a lazy mood tonight...time to crack open another Budweiser.
 
Back
Top